E nānā i nā kumu a me nā hana e hoʻokiʻekiʻe ai i nā hōʻailona o ke kaheʻana i nā hale kūʻai make

Apr 05, 2019

I ka ulu muaʻana,ʻike nā kānaka a pau i kahi e like ai, ae like me nā hōʻailona o ke kaʻe o nā inoa He aha keʻano o ka kahe o ka make o ka make?

ʻO ka hiʻohiʻona nui o nā hōʻailona o nā'āpana o ka makeʻana o nā'āpana make, he mau laina o nā hale o nā hale kūʻaiʻo ka moly

Pehea ka holoʻana o ke kaheʻana o ka makeʻana i ka hanaʻana?

ʻO kekahi mau kumu no ka nānāʻana o ke kaheʻana o ke kahe:

Nā alahele o nā kaulaʻelua o nā kaula haoʻaʻole i hoʻopiliʻia me ka waha;

ʻO ka wela wela ka haʻahaʻa, e like me zinc alloy moll mahana<150 ° C, aluminum alloy mold temperature <180 ° C, are prone to such defects;

He kiʻekiʻe loa ka wikiwiki Hoʻohanaʻia ka coating i ka nui loa {{0}

Pehea e hoʻopau ai i nā kahe nui o ka kahe i nā hewa i ka make?

Kahiki:

Hoʻoponopono i ka wahi o ke keʻahele a i ke kūlana o ka'īpuka; e hoʻoponopono i keʻano o ka mald mahana e hoʻonui ai i ka tank hoʻoponopono i ka wikiwiki e hoʻopiha kūpono pono e hoʻololi i ka moku'āina o keʻano o keʻano o ke kai; ʻO kaʻili a me ka lole a me ka lole {{1}